mixed surprise inspection exposes poor workmanship on khar road bmc slaps 75l fine

Surprise Inspection Exposes Poor Workmanship On Khar Road; Bmc Slaps ?75l Fine

11hrs 4mins   👁 2

Other violations included the use of coarse aggregates of 60mm instead of the required 20mm, and uneven surfaces far beyond the permissible 25mm range. Critically, the mandatory Field Dry Density (FDD) testwhich checks for proper compactionhad not been done, compromising the roads strength and lifespan